Tantalum Rods Bars R05200 Ta1 Ta2 Superalloy Artificial Bone Implant

Place of Origin China
Brand Name Changsheng
Certification ISO 9001;2015
Model Number R05200
Minimum Order Quantity 1kg
Price USD420/kg
Packaging Details Stardard export package
Delivery Time 15-30days
Payment Terms L/C, T/T, Western Union, ,paypal
Supply Ability 500kgs/month
Product Details
Original Place CHINA Packing Standard Wooden Case
Electrical Conductivity 0.13 X 10^6 S/m Process Mixing
Port Tianjin,Qingdao And Shanghai Product Standard ASTM B 365-98
Conditions Annealed Atomic Mass 180.94788 G/mol
Commodity Tantalum Tube Corrosion Resistance Outstanding
Boiling Point 5425°C Specifications Customized
Application Electronics, Chemicals Evaporation Heat 743kJ/mol
Shape Crucible,as Per Drawing
Highlight

Superalloy Tantalum Rods Bars

,

Artificial Bone Implant Tantalum Rods Bars

,

R05200 Tantalum Rods Bars

Leave a Message
Product Description

Description

 

Tantalum rods are rod-shaped products made from tantalum or tantalum-tungsten alloys, commonly supplied in polished finish. Available grades include Ta1 and Ta2, manufactured according to ASTM B365, GB/T26012-2010, or Beijing Oriental Color Tantalum-Niobium enterprise standards.

Key Features:

 

High density: ≥16.6 g/cm³

High melting point: ~3000 °C

Excellent corrosion resistance

Polished surface finish

Customizable dimensions: from Φ0.15 × L, per customer requirements

Applications

Tantalum rods are widely used across multiple industries:

 

Chemical industry: Digesters, heaters, coolers, and corrosion-resistant vessels

Vacuum and high-temperature applications: Blast furnace heating parts, insulation components, and charging vessels

Aerospace & Aviation: Components exposed to extreme heat or corrosive environments

Medical equipment: Devices requiring chemical resistance and biocompatibility

Chemical Composition

Grade Fe Max (%) Si Max (%) Ni Max (%) W Max (%) Mo Max (%) Ti Max (%) Nb Max (%) O Max (%) C Max (%) H Max (%) N Max (%) Ta (%)
Ta1 0.005 0.005 0.005 0.005 0.002 0.002 0.005 0.02 0.004 0.002 0.005 Balance
Ta2 0.005 0.005 0.005 0.005 0.002 0.002 0.1 0.03 0.1 0.002 0.01 Balance